X'inhu S275JR EN 10025 Materjal tal-Azzar Ekwivalenti fiċ-Ċina
S275JR EN 10025 L-azzar huwa azzar ta 'grad strutturali b'saħħa ta' rendiment minimu ta '275 N / mm². S275JR EN 10025 Materjal ekwivalenti tal-azzar fiċ-Ċina huwa l-azzar Q275.

Għal xiex huwa ekwivalenti tal-azzar S275JR?
GB / T 1591-2018 Q275
| Amerikan ASTM / ASME / SAE |
Ewropa en | Ġermanja Din | L-Italja Uni | Franza nf | Ġappun Jis |
|---|---|---|---|---|---|
| A36 | S235J2 | ||||
| A204 Gr. B | 16MO3 | 15mo3 | 16MO3 | 15D3 | |
| A283 A, B, C, D | S185 | ST33 | Fe320 | A33 | SS330 |
| S235jr | St 37-2 | E24-2 | |||
| S235JRG1 | Ust 37-2 | ||||
| A284 Gr. C, d | S235J | St 37-3 n | Fe360d | E24-4 | SM400C |
| S235jr | Rst 37-2 | Fe360b | |||
| S235JO | St 37-3 u | Fe360c | |||
| S235J2+N | St 37-3 n | Fe360d | |||
| A514 | S690Q | Ste690v | E690tr | ||
| A529 Gr. 42, 50 | S275jr | St 44-2 | Fe430b | E28-2 | |
| S275JO | St 44-3 u | Fe430c | E28-3 | ||
| A537 | S460Q | E460tr | SM58 | ||
| A572 Gr. Ċ | S355M | Ste355tm | FEE355KGTM | E355R | |
| A572 Gr. 42 | S275J0 | St 44-3 u | Fe430c | E28-3 | |
| S275J2+N | St 44-3 n | Fe430d | E28-4 | ||
| S275J2 | |||||
| A572 Gr. 50 | S355J2+N | St 52-3 n | Fe510d | E36-3 | SM490C |
| S275J2 | |||||
| A619 | DC03 | ST13 | FEP02 | E | SPCD |
| A620 | DC04 | ST14 | FEP04 | Es | Spce |
| A633 | S355jr | St 52-3 u | Fe510b | E36-2 | SM490A |
| S355JO | Fe510c | E36-3 | SS490 | ||
| A633 Gr. A | S275NL | TSTE285 | |||
| A633 Gr. C, d | S355NL | TSTE355 | FEE355KTN | E355FP | |
| A633 Gr. E | S420NL | TSTE420 | E420fp | ||
| A656 | S335J2 | Fe510dd | E36-4 | SS490YA | |
| S335K2 | |||||
| S335K2+N | |||||
| A70950W | S355J0W | Wtst 52-3 | Fe355W | E36W-B3 | |
| S355J2W | |||||
| S355K2W | |||||
| A945 Gr. 50 | S355ML | TSTE355TM | E355FP | ||
| A945 Gr. 60 | S420ML | TSTE420TM | E420fp | ||
| SA387 Gr. 11 | 13Crmosi 5-5 | ||||
| SA387 Gr. 22 | 10 / 11crmo 9-10 | 10CRMO 9-10 | 12crmo9.10 | 10CD9.10 | |
| Sa516 gr. 55 Sa414 gr. Ċ SA285 Gr. Ċ |
P235GH | Hi | Fe 360-1 kW | A37CP | SPV24 |
| Sa516 gr. 60 Sa414 gr. E |
P265GH | Hii | Fe 410-1 kW | A42CP | SGV42 |
| Sa516 gr. 65 Sa414 gr. F SA299 |
P295GH | 17mn4 | Fe 460-1 kW | A48CP | SGV46 SPV32 |
| Sa516 gr. 70 | P355NH | WSTE355 | Fee355 kW | A510 Ap | |
| P355NL1 | TSTE355 | Fee355 kt | A510 FP | ||
| SAE1020 | C20E | CK20 | C20 | ||
| S275jr | St 44-2 | Fe430b | E28-2 | ||
| S275jr | St 44-2 | Fe430b | E28-2 | ||
| SAE1035 | C35E | CK35 | C35 | XC38 | S35C |
| SAE1040 | C40E | CK40 | C40 | Xc42 | S40C |
| Sae 1042-1045 | C45E | CK45 | C45 | XC48 | S45C |
| SAE4140 SAE4142 |
42CRMO4 | 42CRMO4 | 42CRMO4 | 42CD4 | SCM440H |
| SAE4340 | 34crnimo6 | 34crnimo6 | 34crnimo6 | SNCM447 |
S275JR huwa ekwivalenti għal ASTM A36?
Kemm is-saħħa tar-rendiment kif ukoll is-saħħa tat-tensjoni ta 'l-azzar tal-karbonju S275JR huma ogħla minn dak ta' azzar ħafif ASTM A36. Allura l-azzar tal-karbonju S275JR jista 'jġorr tagħbija itqal minn ASTM ASTM ħafifa A36. Fi kliem ieħor, azzar ħafif ASTM A36 mhuwiex ekwivalenti għall-azzar tal-karbonju S275JR.
S275jr / 1.0044: Propjetajiet skond din en 10 025-2
S275jr|1.0044: Propjetajiet mekkaniċi
| Qawwa tar-rendiment ta 'fuq Reh MPA Min. | Qawwa tat-Tensili RM MPA | Titwil fil-ksur A80% min. | It-titwil fil-ksur ta '5% min. |
|||||
| e inqas minn jew daqs 16 mm | e <3 mm | 3 mm inqas minn jew daqs E inqas minn jew daqs 16 mm | e inqas minn jew daqs 1 mm | 1 mm |
1.5 mm | 2 mm |
2.5 mm | 3 mm inqas minn jew daqs E inqas minn jew daqs 16 mm |
|
| 275 | 430–580 | 410–560 | 13 | 14 | 15 | 16 | 17 | 21 |
S275jr|1.0044: Kompożizzjoni kimika
| Perċentwali bil-piż% massimu. | ||||||
| C | Si | Mn | P | S | N | Cu |
| 0.21 | - | 1.50 | 0.035 | 0.035 | 0.012 | 0.55 |
X'inhu n-numru P għal S275JR ASME?
L-EN S275 JR hija Normalizzazzjoni tal-Europeen (S medju tal-Europ, 275 hija s-saħħa tar-rendiment, JR tfisser 27 J f'20 grad Ċ għat-test tal-impatt), l-ekwivalenti fl-ASME huwa l -SA 572
X'inhu l-ekwivalenti ASTM ta 'S275?
L-ekwivalenti huwaA 520 .
Għal xiex huwa ekwivalenti S275 JR?
| EU EN | USA - | Ġermanja Din, Wnr |
|---|---|---|
| S275jr | A283d A529 Gr.D. | Rst 42-2 st 44-2 |
SS400 huwa ekwivalenti għal S275JR?
B'mod ġenerali,S275JR xi kultant jista 'jintuża bħala alternattiva għal SS400, iżda mhumiex ekwivalenti eżattiJonqos Dejjem ivverifika r-rekwiżiti speċifiċi, peress li xi proġetti jistgħu jeħtieġu konformità ma 'standards speċifiċi (bħal JIS jew EN) li grad wieħed jista' ma jissodisfax għal kollox.
Liema huwa aħjar, S275 jew S355?
L-azzar S355 fih proporzjon ogħla ta 'karbonju meta mqabbel ma' azzar S275 u S235, li jagħmilha aktar b'saħħitha u aktar riġida. Bl-istess mod, S275 Steel fih aktar manganiż minn S235 Steel, li jtejjeb is-saħħa u l-ebusija tiegħu.
S235JR huwa ekwivalenti għal S275JR?
S235JR għandu saħħa minima ta 'rendiment ta' 235 MPa, filwaqt li S275JR għandu saħħa ta 'rendiment minima ta' 275 MPa. Dan ifisser li S275JR huwa aktar b'saħħtu minn S235JR u tipikament jintuża għal applikazzjonijiet aktar impenjattivi, bħal makkinarju tqil, bini għoli, u strutturi kbar.
X'inhi d-differenza bejn S355 JR u S275 JR?
S275JR huwa l-azzar tal-karbonju, filwaqt li S355JR huwa azzar baxx tal-ligaJonqos Kemm l-azzar tal-karbonju S275JR kif ukoll l-azzar tal-liga baxxa S355JR huma taħt l-istandard EN 10025-2. L-azzar tal-liga baxxa S355JR huwa grad tal-azzar ogħla minn azzar tal-karbonju S275JR.