X'inhu l-grad S275J2 (1.0145)?
Grad S275J2 għanduQawwa minima tar-rendiment ta '275 MPaJonqos L-enerġija tal-impatt f'temperatura tat-test ta '-20 grad hija mill-inqas 27 joules.
X'inhi d-differenza bejn S275J2 u S355J2?
S355jr vs S355J2: għandu ebusija aħjar peress li huwa ttestjat fi -20 grad meta mqabbel ma 'S355JR, li huwa ttestjat f'20 grad.
S355J2 vs S275J2: S355J2 għandu saħħa ogħla (355 MPa) meta mqabbel ma 'S275J2 (275 MPa).
Kompożizzjoni kimika ta 'azzar strutturali - S235, S275 u S355
| Grad | C% | Mn% | P% | S% | Si% |
| S235 | 0. 22 Max | 1.60 Max | 0. 05 Max | 0. 05 Max | 0. 05 Max |
| S275 | 0. 25 Max | 1.60 Max | 0. 04 Max | 0. 05 Max | 0. 05 Max |
| S355 | 0. 23 Max | 1.60 Max | 0. 05 Max | 0. 05 Max | 0. 05 Max |
Qawwa tar-rendiment ta 'l-azzar strutturali - S235, S275, S355
| Grad strutturali tal-azzar f'16mm | Qawwa minima tar-rendiment bi ħxuna nominali 16mm | |
| KSI | N / mm 2 (MPA) | |
| S235 | 33 000 ksi | 235 N / mm 2 |
| S275 | 36 000 ksi | 275 N / mm 2 |
| S355 | 50 000 ksi | 355 N / mm 2 |
Qawwa tat-tensjoni ta 'l-azzar strutturali - S235, S275, S355
| Grad strutturali tal-azzar | Qawwa tat-Tensili MPA fil-ħxuna tan-nom bejn 3mm u 16mm |
| S235 | 360 - 510 MPA |
| S275 | 370 - 530 MPA |
| S355 | 470 - 630 MPA |
X'inhi d-differenza bejn 275Jr u 275J2?
Id-differenza ewlenija fost it-tliet azzar S275 tinsab fit-temperatura tal-impatt tagħhom: 2 0 grad ta 'azzar S275jr, -20 grad ta' azzar S275J2 u {0 grad ta 'S275J0 azzar.
S275J2 (1.0145) Standard Ċina ekwivalenti
Q275D
Iċ-Ċina Standard Ekwivalenti għall-Grad tal-Azzar Ewropew S275J2 huwaGB / T 1591-2018 Q275DJonqos S275J2, skond EN 10025-2, huwa azzar strutturali mhux liga b'qawwa ta 'rendiment minimu ta' 275 MPa. L-istandard Ċiniż Q275, misjub fi GB / T 700, huwa wkoll azzar strutturali bi proprjetajiet simili.
| Eu En |
Ingilterra BS |
Xjuħ Ewropew En |
Belġju NBN |
Iċ-Ċina Gb / t 1591-2018 |
L-Iżvezja Ss |
L-Indja IS |
|||||||